If the profile wall thickness tolerance allows, file or sand the surface of the working belt of the mold core; if the degree of wear of the working belt of the mold core is severe and the profile wall thickness has reached the upper deviation,replace the mold , repair the shape of the mold core, file it to the required size and polish it before use; if the core working belt is not worn out, file the outer obstruction and the inner detention area of the core working belt.